Low moisture recovery rods (LMA) for mild and low alloy steels. In rising vertical, where welding speed is high. Welding current: DC + (-). Stretching: 29 %. Charge de rupture : 540 Mpa. Limite d'élasticité : 445 Mpa. Cadence de dépôt : 125 %. Steaming time: less than 2 hours.